Mechanical Properties Metric English Comments
Tensile Modulus 0.662 GPa
96.0 ksi
ASTM D638
Ecomass® 4703ZD88 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym..
Tensile Modulus 0.662 GPa
96.0 ksi
ASTM D638
Ecomass® 4703ZD95 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Po..
Tensile Modulus 0.662 GPa
96.0 ksi
ASTM D638
Ecomass® 4703ZG92 Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers