Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.670 GPa | 97.2 ksi | ISO 527-2 |
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Tensile Modulus | 0.670 GPa | 97.2 ksi | ISO 527-2 |
Solvay Specialty Polymers Polidan® T/A-SP Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-SP is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |