Polymer Property : Tensile Modulus = 0.778 GPa
Polymer Property :
Tensile Modulus =
0.778 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Modulus
0.778
GPa
113
ksi
chs 2.0 in/min; ASTM D638
Diamond Polymers ABS 9950 Injection Molding Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.