Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00586 GPa | 0.850 ksi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 0883-01 RoHS BLACK Polyethylene, Chlorinated (CPE) CPE-0833-1 RoHS BLACK is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-0833-1 RoHS BLACK offers the highest level of fi.. |