Tensile Modulus 0.870 GPa
126 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON FX98500 PE
LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Modulus 0.870 GPa
126 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Tensile Modulus 0.870 GPa
126 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON PE002Z PA 6
LNP* STAT-KON* PE002Z is a compound based on Nylon 6 resin containing 10% Carbon Fiber. Added features of this grade include: Extrusion Grade.
Tensile Modulus 0.870 GPa
126 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific)
LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Tensile Modulus 0.870 GPa
126 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON FX98500C PE