Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.905 GPa | 131 ksi | 1 mm/min |
Arkema Group Appryl® 7280 Polypropylene - Polyethylene Copolymer PP/PE copolymer colored directly or during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive i.. |