Mechanical Properties Metric English Comments
Tensile Modulus 0.920 GPa
133 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR
LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Tensile Modulus 0.920 GPa
133 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific)
LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Tensile Modulus 0.920 GPa
133 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Tensile Modulus 0.920 GPa
133 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR (Asia Pacific)
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Tensile Modulus 0.920 GPa
133 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I
Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril..