Mechanical Properties Metric English Comments
Tensile Modulus 1.07 GPa
155 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Stat-Tech™ ST5220-0004 CP4D EG Black Polypropylene Impact Copolymer (PP Impact Copolymer)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Tensile Modulus 1.07 GPa
155 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON FX98500 PE
LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Modulus 1.07 GPa
155 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Tensile Modulus 1.07 GPa
155 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific)
LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Tensile Modulus 1.07 GPa
155 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON FX98500C PE
LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Modulus 1.07 GPa
155 ksi
MD, 2% Secant; ASTM D882
Dow INSPIRE™ D118.01 Developmental Performance Polymer
D118.01 Developmental Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion. Film and sheet produced from this resin offer improved stiffness, heat resistance, ..
Tensile Modulus 1.07 GPa
155 ksi
1 mm/min
Arkema Group Rilsan® BMN D Nylon 11 (Conditioned)
Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d..
Tensile Modulus 1.07 GPa
155 ksi
Addcomp PRIEX® 11002 Maleic Anhydride Grafted HDPE
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..
Tensile Modulus 1.07 GPa
155 ksi
Addcomp PRIEX® 11006 Maleic Anhydride Grafted HDPE
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..