Polymer Property : Tensile Modulus = 1.107 GPa
Polymer Property :
Tensile Modulus =
1.107 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Modulus
1.107
GPa
160.6
ksi
1mm/min; ISO 527
BASF Ultramid® B3S Q661 PA6 (Dry)
Ultramid B3S Q661 is a general purpose, PA6 resin for injection molding.