Mechanical Properties Metric English Comments
Tensile Modulus 1.19 GPa
173 ksi
ASTM D638
Quadrant EPP Proteus® PP, Black Homopolymer Polypropylene (ASTM Product Data Sheet)
High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion..
Tensile Modulus 1.19 GPa
173 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP FARADEX MS003 PP
LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Tensile Modulus 1.19 GPa
173 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Tensile Modulus 1.19 GPa
173 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Tensile Modulus 1.19 GPa
173 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific)
A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications
Tensile Modulus 1.19 GPa
173 ksi
ASTM D638
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet)
Tensile Modulus 1.19 GPa
172 ksi
ASTM D638
Styron INSPIRE™ TF3800 Polypropylene
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010