Mechanical Properties Metric English Comments
Tensile Modulus 0.00869 GPa
1.26 ksi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W2402 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Copyright © lookpolymers.com All Rights Reserved