Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.32 GPa | 191 ksi | Tangent Method; ASTM D638 |
Ineos N10N-00 Polypropylene Impact Copolymer Grade N10N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and .. |
|||
Tensile Modulus | 1.32 GPa | 191 ksi | ASTM D638 |
Ineos N12N-00 Polypropylene Impact Copolymer Grade N12N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and .. |
|||
Tensile Modulus | 1.32 GPa | 192 ksi | ISO 527-2/1 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Tensile Modulus | 1.32 GPa | 191 ksi | ISO 527-2/1 |
ExxonMobil PP7684KN Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance .. |
|||
Tensile Modulus | 1.32 GPa | 192 ksi | ASTM D638 |
Arkema Group Solarkote® P-610 Acrylic PVC Capstock, clear, low glossInformation provided by Arkema Group |