Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.34 GPa | 195 ksi | 1% Secant; 0.5"/min; ASTM D638 |
LyondellBasell Lupolen® 5261 Z Q 456 B High Density Polyethylene, Pipe and Sheet Extrusion Grade Lupolen 5261 Z Q 456 B is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 um) p.. |
|||
Tensile Modulus | 1.34 GPa | 194 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber PA 6, injection molding grade, 10% glass fibers/mineral, good heat-ageing resistance |
|||
Tensile Modulus | 1.34 GPa | 194 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 1.34 GPa | 194 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Tensile Modulus | 1.34 GPa | 194 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |
|||
Tensile Modulus | 1.34 GPa | 194 ksi | ISO 527-2 |
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes Polypropylene PPC 1640 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It exhibits high stiffness in co.. |
|||
Tensile Modulus | 1.34 GPa | 194 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMU130P Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci.. |
|||
Tensile Modulus | 1.34 GPa | 194 ksi | ASTM D638 |
Arkema Group Solarkote® P-601 Acrylic PVC Capstock, white, high glossInformation provided by Arkema Group |
|||
Tensile Modulus | 1.34 GPa | 194 ksi | 1 mm/min |
Arkema Group Rilsan® BESHV Nylon 11, Blow Molding Grade (Conditioned) Designation ISO 1874-PA11,E,24-010Rigid grade for extrusion blow molding. Available color: natural. Additive free.Very good impact strength. Well adapted melt strength. High chemical resistance.Food.. |