Mechanical Properties Metric English Comments
Tensile Modulus 1.4166 GPa

@Temperature 170 °C
205.46 ksi

@Temperature 338 °F
50%RH; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..