Tensile Modulus 1.475 GPa
213.9 ksi
XY direction; ASTM D638
ALM PA 860 White Nylon 11 SLS Prototyping Polymer
Unfilled White PA 11 that is formulated for easy processing across all LS platforms. Tightly controlled particle distribution creates a smooth surface finish and excellent feature detail. Parts prod..