Mechanical Properties Metric English Comments
Tensile Modulus 1.724 GPa
250.0 ksi
ASTM D638
Ineos Styrenics Polystyrene 476M (NAFTA)
High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF ..