Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.744 GPa | 252.9 ksi | ASTM D638 |
RedEye On Demand PC-ISO for Parts that can be Sterilized Polycarbonate-ISO (PC-ISO) is a durable high-performance plastic that meets both ISO 10993-1 and USP Class VI standards in its raw state. PC-ISO can be sterilized using either the gamma radiation or.. |
|||
Tensile Modulus | 1.744 GPa | 252.9 ksi | Type 1, 2"/min; ASTM D638 |
Stratasys® Polycarbonate-ISO PC-ISO (polycarbonate-ISO), an industrial thermoplastic, in its raw state meets the ISO 10993-1 and USP Class VI classification1 and comes in a variety of colors. Because of their strength and medic.. |