Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.863 GPa | 270.2 ksi | |
Kuraray HYBRAR® PS1 Thermoplastic Rubber-Polystyrene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |