Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1.875 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.875 GPa
271.9 ksi
cast films MD; ISO 527-3
Borealis Bormod™ HC904CF Polypropylene
Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech..
Copyright © lookpolymers.com All Rights Reserved