Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1.89 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0130 GPa
1.89 ksi
ISO 527
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tensile Modulus 0.0130 GPa
1.89 ksi
ISO 527
Polyram PlusTek PB202G50BK39 Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized
50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by NSF/ANSI 61 International.Information provided by Polyram.
Tensile Modulus 0.0130 GPa
1.89 ksi
1 mm/min
Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..
Copyright © lookpolymers.com All Rights Reserved