Mechanical Properties Metric English Comments
Tensile Modulus 10.38 GPa
1505 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI
LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber.