Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 10.498 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 10.498 GPa

@Temperature -20.0 °C
1522.6 ksi

@Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided ..