Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 7.47 GPa
1080 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica..
Tensile Modulus 7.45 GPa
1080 ksi
ASTM D638
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h..
Tensile Modulus 7.45 GPa
1080 ksi
ASTM D638
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h..
Tensile Modulus 7.42 GPa
1080 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific)
Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade.
Tensile Modulus 7.446 GPa
1080 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK
LNP* THERMOCOMP* LF003 is a compound based on Polyetheretherketone resin containing 15% Glass Fiber.
Tensile Modulus 7.446 GPa
1080 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific)
LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Tensile Modulus 7.47 GPa
1080 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6
LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat.
Tensile Modulus 7.45 GPa
1080 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF)
LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Tensile Modulus 7.46 GPa

@Temperature 60.0 °C
1080 ksi

@Temperature 140 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Tensile Modulus 7.44 GPa
1080 ksi
50 mm/min; ASTM D638
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded
PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo..
Tensile Modulus 7.43 GPa
1080 ksi
1 mm/min
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid..
Tensile Modulus 7.47 GPa
1080 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific)
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated.