Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.14 GPa | 1616 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 11.14 GPa | 1616 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific) LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber. |