Tensile Modulus 11.32 GPa
1642 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DE003Z PC
LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Extrusion Grade.