Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.66 GPa | 1110 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
Tensile Modulus | 7.64 GPa | 1110 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 7.64 GPa | 1110 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 7.64 GPa | 1110 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Tensile Modulus | 7.68 GPa | 1110 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold .. |
|||
Tensile Modulus | 7.68 GPa | 1110 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific) LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret.. |
|||
Tensile Modulus | 7.65 GPa | 1110 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant. |
|||
Tensile Modulus | 7.66 GPa | 1110 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
Tensile Modulus | 7.63 GPa | 1110 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific) LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 7.64 GPa | 1110 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66 LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 7.64 GPa | 1110 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 7.65 GPa | 1110 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 7.65 GPa | 1110 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF VF006U Super Tough Nylon LNP* Thermotuf* VF006U is a compound based on Super Tough Nylon containing Glass Fiber. Characteristics of this grade are High Impact. |
|||
Tensile Modulus | 7.65 GPa @Temperature 40.0 °C |
1110 ksi @Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Modulus | 7.67 GPa | 1110 ksi | ISO 527 |
Azdel AZMET® CM32350 35% continuous random fiber mat / PET resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polyethylene Terephthalate (PET) resin matrix. This composite material fea.. |