Polymer Property : Tensile Modulus = 12.33 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 12.33 GPa
1788 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific)
LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Tensile Modulus 12.33 GPa
1788 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon EE005 PEI
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Tensile Modulus 12.33 GPa
1788 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific)
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Tensile Modulus 12.33 GPa
1788 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON EE005E PEI
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Tensile Modulus 12.33 GPa
1788 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON EE005E PEI (Asia Pacific)
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Tensile Modulus 12.33 GPa
1788 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Asia Pacific)
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 12.33 GPa
1788 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..