Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.837 GPa @Temperature 30.0 °C |
121 ksi @Temperature 86.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |