Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 85.4 GPa @Temperature 23.0 °C |
12400 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form Fiber: IM7-12KInformation provided by HexCel |