Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.862 GPa | 125 ksi | 1% Secant; 50mm/min; ASTM D638 |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Tensile Modulus | 0.862 GPa | 125 ksi | ASTM D638 |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |
|||
Tensile Modulus | 0.862 GPa | 125 ksi | ASTM D638 |
Westlake Plastics Kynar® 2850 PVDF Copolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Tensile Modulus | 0.860 GPa @Temperature 80.0 °C |
125 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |