Mechanical Properties Metric English Comments
Tensile Modulus 0.8680 GPa
125.9 ksi
1% Secant; 50mm/min; ASTM D638
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade
ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c..