Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.39 GPa | 2087 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 14.39 GPa | 2087 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450EX PBT (Asia Pacific) LNP* Thermocomp* WH0450EX is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 14.39 GPa | 2087 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT (Asia Pacific) LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |