Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 140 GPa | 20300 ksi | Longitudinal tensile test (fiber direction)_These values are normalized to 60% of fiber volume fraction; ASTM D3039 |
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the.. |
|||
Tensile Modulus | 140 GPa | 20300 ksi | Vf=59% |
Toyobo Zylon® HM Fiber/Epoxy Matrix Unidirectional Composite Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using the latest material science and state of the ar.. |
|||
Tensile Modulus | 140 GPa @Temperature 23.0 °C |
20300 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix, Unidirectional Prepreg Laminate (M36/32%/135/HTA) Tenax HTA fiberInformation provided by HexCel |