Tensile Modulus 10.32 GPa
1497 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12
LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber.
Tensile Modulus 10.32 GPa
1497 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..
Tensile Modulus 10.32 GPa
1497 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66
LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding.
Tensile Modulus 10.32 GPa
1497 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas ..