Polymer Property : Tensile Modulus = 15.31 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 15.31 GPa
2221 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 (Asia Pacific)
LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.