Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.7 GPa @Temperature 23.0 °C |
2280 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 BK851 PBT
(Unverified Data**) Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 15.7 GPa | 2280 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Tensile Modulus | 15.7 GPa | 2280 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Tensile Modulus | 15.7 GPa | 2280 ksi | |
LATI Latiohm 80-05 CNT GCE/500 PPS, Glass/Mineral Reinforced Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Carbon nanotubes. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Tensile Modulus | 15.7 GPa | 2280 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Tensile Modulus | 15.7 GPa | 2280 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK609 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**) 50% Glass Reinforced Polybutylene Terephthalate Crastin SK609 BK851 is a 50% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |