Mechanical Properties Metric English Comments
Tensile Modulus 10.64 GPa
1543 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc..
Tensile Modulus 10.64 GPa
1543 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® FR50 BK505 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 BK505 is a 25% glass fiber reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Perfo..