Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 159 GPa | 23000 ksi | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-256-T(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0408-155HTInformation Provided by Pacific Sintered Metals, a divis.. |
|||
Tensile Modulus | 159 GPa | 23100 ksi | Typical epoxy composite property |
Hexcel® HexTow™ IM6 Carbon Fiber HexTow™ IM6 carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized .. |
|||
Tensile Modulus | 159 GPa @Temperature 23.0 °C |
23100 ksi @Temperature 73.4 °F |
0° |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, G40-800 Fiber Information provided by HexCel |