Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | >= 0.120 GPa | >= 17.4 ksi | MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | >= 0.120 GPa | >= 17.4 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | >= 0.120 GPa | >= 17.4 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | >= 0.120 GPa | >= 17.4 ksi | 2% sec, TD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | >= 0.120 GPa | >= 17.4 ksi | 2% sec, TD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | >= 0.120 GPa | >= 17.4 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | 0.120 GPa | 17.4 ksi | ISO 527-1/-2 |
Styrolution Styroflex® 2G 66 SBC Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o.. |
|||
Tensile Modulus | 0.120 GPa | 17.4 ksi | ISO 527-1/-2 |
DSM Arnitel® PM460-H TPC-ET Injection Molding, Heat Stabilized |
|||
Tensile Modulus | 0.120 GPa | 17.4 ksi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |