Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.81 GPa | 2583 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 LNP* THERMOCOMP* RF00AH is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 17.81 GPa | 2583 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 (Asia Pacific) LNP* Thermocomp* RF00AH is a compound based on Nylon 66 resin containing Glass Fiber. |