Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.800 - 1.20 GPa | 116 - 174 ksi | DIN 53457 |
Isoflon PVDF Polyvinyl Dichloride Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Modulus | 0.800 - 1.20 GPa | 116 - 174 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Tensile Modulus | 0.800 - 1.20 GPa @Thickness 2.00 mm, Temperature 23.0 °C |
116 - 174 ksi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 0.500 - 1.20 GPa | 72.5 - 174 ksi | DIN 53457 |
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |