Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.5 - 12.0 GPa | 1520 - 1740 ksi | ISO 527 |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |