Tensile Modulus 1.22 GPa
177 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON MD000 PP
LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive.
Tensile Modulus 1.22 GPa
177 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific)
LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Tensile Modulus 1.22 GPa
177 ksi
1mm/min; ISO 527
BASF Ultramid® 8202CQ PA6 (Conditioned)