Mechanical Properties Metric English Comments
Tensile Modulus 12.38 GPa
1796 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV0079 PA 66
LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural.