Tensile Modulus
18.68
GPa
2709
ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA6.10
LNP* THERMOCOMP* QF00A is a compound based on Nylon 6/10 containing 50% Glass Fiber.