Polymer Property : Tensile Modulus = 18.79 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 18.79 GPa
2725 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI
LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by ..
Tensile Modulus 18.79 GPa
2725 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific)
LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by ..