Polymer Property : Tensile Modulus = 18.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 18.8 GPa
2730 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr..
Tensile Modulus 18.8 GPa
2730 ksi
5 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl..
Tensile Modulus 18.8 GPa
2730 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 (Europe-Africa-Middle East)
LNP* Thermocomp* RF00C is a compound based on Nylon 66 resin containing Glass Fiber.