Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.5 GPa | 1810 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 66 GF 35 Polyamide 66, 35% Glass Fiber FeaturesChemically reinforced with 35% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527 |
Nilit FRIANYL A63 HH-GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527-2 |
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 - 1/2 |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527-1/-2 |
Lanxess Durethan® BCF 30 X H2.0 901510 Nylon 6, 30% Glass + Carbon Fiber PA 6, injection molding grade, 30% reinforced (glass fibers + carbon fibers), conductive, intrinsic color black, good heat-ageing resistance |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® TP 036-052 000000 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, good flowability (Easy Flow), good heat-resistance |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon AE004E ABS LNP* Stat-Kon* AE004E is an ABS compound containing Glass Fiber. Characteristics of this grade are Statically Conductive and Easy Molding.This data was supplied by SABIC-IP for the Americas region... |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V9280LW PET (Europe-Africa-Middle East) 40% Glassfiber / Mineral Filled PET, Impact Modifier, Mold Release, Heat StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific) LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66 LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 12.5 - 14.0 GPa | 1810 - 2030 ksi | ISO 527 |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® AG-35 PA66-GF35 Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® SC50 PA46-GF30 FR 30% Glass Reinforced, Flame Retardant, Halogen free and free of red phosphorous |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVZ 45 HWCP 45% Glass Fiber Nylon 6, Impact Resistant, Good Surface Finish, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 12.5 GPa @Temperature 120 °C |
1810 ksi @Temperature 248 °F |
ISO 527-1/-2 |
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-50-4 nat PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40 Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4108 black 9992 PA612-GF50 Product description: Grilamid XE 4108 black 9992 is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorpti.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4108 nat PA612-GF50 Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | same value from ASTM and ISO test. |
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50 Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TRVX-50X9 black 9230 PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |
|||
Tensile Modulus | 12.5 GPa | 1810 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TRVX-50X9 nat PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |