Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.56 GPa | 1822 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |