Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 186 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 186 GPa
27000 ksi
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable
Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that..
Tensile Modulus 186 GPa
27000 ksi
filament
3M Nextel™ BF-30 Woven Fabric 440
Information provided by 3M
Tensile Modulus 186 GPa
27000 ksi
filament
3M Nextel™ BF-20 Woven Fabric 440
Information provided by 3M
Tensile Modulus 186 GPa
27000 ksi
filament
3M Nextel™ BF-40 Woven Fabric 440
Information provided by 3M
Tensile Modulus 186 GPa
27000 ksi
Young's; DINV ENV 843-2 / ASTM-F417
CeramTec 848 Zirconia, ZrO2•MgO
Tetragonal zirconia exhibits high flexural strength and superior low temperature stability. It features higher impact strength and erosive wear resistance as compared to alumina. 848 TTZP (yellow) i..